OxyPars series for Fluidized Bed

Our 4th generation Oxypars catalyst is designed and manufactured based on an extensive research. it has been successfully applied in commercial units such as Arvand and Abadan petrochemical companies

 4th generation OxyPars series for Fluidized Bed

-Improved HCl conversion rate -

More EDC purity -

Low combustion rate-

-Low stickiness -

Low Catalyst lost rate -

Low Attrition rate-

Type

4th generation

Form

Micro spherical powder

                                  <30µm

Size                       30-120  µm

>120 µm

15%

82%

3 %

Color

yellow

BET Surface Area     (m2/g)

110-150

Total Pore Volume   (cm3/g)

0.15-0.35

                                 %  Al2O3

Balance

                                  %    Cu  

4-4.5

Promoters

Variant

 

 

 

1st , 2nd and 3rd Generation Oxypars Series 

Type

NP- 100

NP- 200

NP- 300

Form

Micro spherical powder

Micro spherical powder

Micro spherical powder

Average size

50-80(µ)

40-90(µ)

40-90(µ)

Color

Green

Yellow

Yellow

Surface Area             (m2/g)

120-180

100-160

100-170

                                 %  Al2O3

Balance

Balance

Balance

                                  %    Cu  

9-13

3.5-4.2

3.5-5

Promoters

Variant

Variant

Variant

We have the capacity to produce this product with different parameters